Standard:API 5L PSL 2, 46. utgave

Stålkvalitet:

1) Sømløs rørledning for generell service

BN/L245N, X42N/L290N, X46N/L320N, X52N/L360N, X52Q/L360Q, X56N/L390N, X60N/L415N, X60Q/L415Q, X65Q/L450Q, X5Q, X5Q, X5Q, X5Q X90Q/L625Q

2) Sømløs linjerør for sur service

BNS/L245NS, X42NS/L290NS, X46NS/L320NS, X52NS/L360NS, X52QS/L360QS, X56NS/L390NS, X60QS/L415QS, X65QS/L450QS, X70QS/L4

3) Sømløs rørledning for havservice

BNO/L245NO, X42NO/L290NO, X46NO/L320NO, X52NO/L360NO, X52QO/L360QO, X56NO/L390NO, X60QO/L415QO, X65QO/L450QO, X705QO/L5Q, X805QO/L5Q X90QO/L625QO.

4) Sveiset ledningsrør for generell service

BR/L245R, L290R/X42R, L245N/BN, L290N/X42N, L320N/X46N, L360N/X52N, L390N/X56N, L415N/X60N

BQ/L245Q, L290Q/X42Q, L320Q/X46Q, L360Q/X52Q, L390Q/X56Q, L415Q/X60Q, L450Q/X65Q, L485Q/X70Q, L555Q/X80Q, L90Q/X50Q, L6Q.

BM/L245M, L290M/X42M, L320M/X46M, L360M/X52M, L390M/X56M, L415M/X60M, L450M/X65M, L485M/X70M, L555M/X80M,

L625M/X90M, L690M/X100M.

5) Sveiset linjerør for sur service

 

BMS/BNS/BQS/L245MS/L245NS/L245QS, L290MS/L290NS/L290QS/X42MS/X42NS/X42QS, L320MS/L320NS/L320QS/X46MS/X46NS/X46QS, L360MS/L360NS/L360QS/X52MS/X52NS/X52QS, L390MS/L390NS/L390QS/X56MS/X56NS/X56QS, L415MS/L415NS/L415QS/X60MS/6X60S, L450MS/L450NS/L450QS/X65MS/X65NS/X65QS, L485MS/L485NS/L485QS/X70MS/X70NS/X70QS, L555MS/L555NS/L55QS/X80MS/X80QNS

Størrelsesområde:

OD: 21,3-1422mm WT: 2-60mm Lengde: 5,8m, 6m, 11,8m, 12m eller i henhold til kundenes krav.

Andre standarder:

Kina: GB/T 9711-2017
ISO: ISO 3183-2012, NACE MR0175/ISO 15156
SHELL Standard: DEP 31.40.20.37
TOTAL Standard: TOTAL GS EP PLR 201
Canada Standard: CSA Z245.1-14
Kuwait Standard: KOC-MS-001 PT.1 REV.2(2009), KOC-MS-018
Norge Standard: DNV-OS-F101

Produksjonsprosess: Sømløs, LSAW, JOCE, UOE, RBE

Pakke: Fasede eller rette ender med plasthetter eller metallbeskyttere, svartmalt, sekskantet buntet eller løs pakning.

Bruk: Vannrørledning, petroleumsrørledning, bensinrørledning, oljeterminalrørledning, oljekaierørledning.

Kjemisk sammensetning og mekaniske egenskaper for API 5L PSL2 linjerør:

API 5L RØR
PSL2

Kjemisk sammensetning

Mekanisk eiendom

C (maks.)

Mn (maks.)

P (maks)

S (maks)

Strekk

Avkastning C. E. PÅVIRKNING ENERGI

Psi x 1000

Mpa

Psi x 1000

Mpa PCM IIW J FT/LB

Karakter B

0.22

1.20

0.025

0.015

60 – 110

414 – 758

35 – 65

241 – 448

0.25

0.43

T/L 27/41

T/L 20/30

Karakter X42

0.22

1.30

0.025

0.015

60 – 110

414 – 758

42 – 72

290 – 496

0.25

0.43

T/L 27/41

T/L 20/30

Karakter X46

0.22

1.40

0.025

0.015

63 – 110

434 – 758

46 – 76

317 – 524

0.25

0.43

T/L 27/41

T/L 20/30

Karakter X52

0.22

1.40

0.025

0.015

66 – 110

455 – 758

52 – 77

359 – 531

0.25

0.43

T/L 27/41

T/L 20/30

Karakter X56

0.22

1.40

0.025

0.015

71 – 110

490 – 758

56 – 79

386 – 544

0.25

0.43

T/L 27/41

T/L 20/30

Karakter X60

0.22

1.40

0.025

0.015

75 – 110

517 – 758

60 – 82

414 – 565

0.25

0.43

T/L 27/41

T/L 20/30

Karakter X65

0.22

1.45

0.025

0.015

77 – 110

531 – 758

65 – 82

448 – 565

0.25

0.43

T/L 27/41

T/L 20/30

Karakter X70

0.22

1.65

0.025

0.015

82 – 110

565 – 758

70 – 82

483 – 565

0.25

0.43

T/L 27/41

T/L 20/30

Karakter X80

0.22

1.90

0.025

0.015

90 – 120

621 – 827

80 – 102

552 – 705

0.25

0.43

T/L 27/41

T/L 20/30

 

Vennligst oppgi informasjonen nedenfor hvis du ber om tilbud:

Tittel

API 5L Line Pipe

Antall

Stk/Mtr/tonn

Størrelse

NPS (ytterdiameter) og tidsplan nr. (veggtykkelse) og lengde

PSL-nivå

PSL 1 eller PSL 2

Karakter

Grade A, Grade B, X42, X46, X52, X60, X70, X80 osv.

Produksjonsprosess

Sømløs eller sveiset

Overflatefinish

Bar, svart

Slutter finish

Vanlige ender, skrå ender, gjengede ender

Hvis forskjellig fra API 5L-spesifikasjonen

Beskyttende belegg og foringer

3LPE, 3LPP, FBE, AkzoNobel, epoksy sinkrik grunning, flytende epoksyharpiks, etc.

Produsent

Godkjent produsentliste (AML), eller restriksjoner for opprinnelsesland

Sur service

Ja / Nei

 

info-290-174

Sende bookingforespørsel

whatsapp

Telefon

E-post

Forespørsel